The ABS luggage process mainly includes the following steps:
Material preparation: Select appropriate ABS plastic sheets to ensure that their thickness and color meet the requirements.
Heating and softening: Place the ABS sheet in an oven and heat it to the softening temperature, usually 140-160℃.
Molding: Place the softened sheet on the mold and fit it to the mold shape through vacuum adsorption to form the desired luggage shape.
Cooling and shaping: Use air cooling or water cooling to solidify the molded parts to ensure stable shape.
Subsequent processing: The molded luggage is trimmed and surface treated, such as polishing, painting, etc., to improve appearance and durability.